I've had some problems with this with my kiln in my studio, with most of the reduction disappearing, but I haven't had that problem when I'm working at the studio at BeadFX. I read a tip about annealing / garaging at a lower temperature. So I turned the garage temperature down to 950, and the post gaaging to 925F, I left the rest of the cycle the same and I am getting much, much better results. Much happier now.